How to fix bubbly acrylic resin?

If you’ve ever worked with acrylic resin, you know how disheartening it is to pull a finished project out of its mold only to see those pesky, ragged bubbles scattered across the surface. As an acrylic resin supplier, I get dozens of messages every week from hobbyists, small makers, and even furniture repair shops asking, “Why are my bubbles there, and how do I fix them without ruining the piece I spent hours on?” I’ve been selling and advising on resin for over seven years, and I’ve worked through every kind of bubbly mess—from tiny pinholes in keychains to large surface bubbles on countertop casts. The good news is that fixing bubbly acrylic resin isn’t as complicated as it sounds, and many issues can be avoided before they even start. Let’s break this down step by step, from identifying the root causes of bubbles to repairing existing ones and preventing them for good. Acrylic Resin

First, I need to be clear: not all bubbly resin is the same. The bubbles you see fall into two main categories, and how you address them depends on which one you’re dealing with. Pinhole bubbles are tiny, almost microscopic indentations that dot the surface—these usually pop up within a few minutes of pouring, caused by air trapped in the resin mixture. Surface bubbles are larger, round or irregularly shaped pockets that sit just below or on the resin’s top layer, often forming when you pour resin too quickly or don’t work the mixture enough to release air. I’ve seen new makers mix their resin too fast to save time, and that’s the number one reason for pinholes. The chemical reaction between resin and hardener is exothermic, meaning it creates heat, and rushing that process traps air that can’t escape.

Before we get to fixes, though, let’s talk about when it’s too late to repair a bubble entirely. If a bubble is big enough to cause structural weakness in a piece—say, a edge of a resin tabletop that has a two-inch air pocket running through it—you won’t be able to patch it effectively without sanding down that section entirely and re-pouring resin. That’s a last-resort fix, and I’ll cover that later. For most small to medium projects, though, whether it’s a resin art tray, a handle for a tool, or a set of coasters, bubbly resin is fixable with a few simple tools.

Let’s start with the most common scenario: bubbles that have just formed, within the first 15 to 30 minutes after pouring. This is the sweet spot for fixing them, because the resin is still in a “green” state—it’s no longer liquid, but it hasn’t fully cured yet, so it’s malleable enough to work with. The tools you’ll need here are cheap and probably already in your workshop or kitchen: a butane torch (not a regular kitchen lighter, which doesn’t have enough heat), a heat gun, a sanding sponge, and a small, flat wooden stick. I tell all my customers to keep a torch on hand for this exact reason. When I’m at the shop, if someone calls panicking about bubbles in a test pour, my first question is always, “Do you have a butane torch?” Most of the time, the answer is yes.

The method here is straightforward: hold the torch about 6 to 8 inches away from the resin’s surface, moving it slowly in a circular motion. Don’t hold it in one spot too long—you’ll overheat the resin, cause discoloration, or even burn the surface. The heat from the torch doesn’t melt the resin, it lowers its viscosity, which makes trapped air bubbles rise to the surface and pop. You’ll see tiny ripples form on the resin as each bubble breaks; keep moving the torch until all the bubbles have dissipated. For pinholes, this method works especially well because the heat is just enough to pop each tiny air pocket without leaving a mark. After the resin cures, you can sand the surface lightly to smooth out any slight texture, and it’ll look almost as good as a bubble-free pour.

If you don’t have a torch, a heat gun on its lowest setting works too, but you have to be even more careful. Heat guns can blow air, which might create new bubbles if you’re too close, so keep it at least a foot away from the surface. Another DIY alternative is using a hair dryer on its hottest setting—though this takes longer, usually 5 to 10 minutes, and I don’t recommend it for larger projects. I’ve had a customer once use a hair dryer for a large resin clock face, and the bubbles didn’t pop all the way because the heat was uneven across the surface. Stick to a torch for the best results, and make sure it’s one designed for soldering or cooking—regular craft torches often don’t get hot enough.

Now, what if the bubbles didn’t pop when the resin was still green? That means they’re cured—fully hard, set resin with air pockets trapped inside. This is the more tricky fix, because you have to work with a solid surface instead of a soft, workable one. Again, we split this into small surface bubbles and larger structural bubbles. For small surface bubbles, like pinholes or bubbles less than a quarter inch wide, here’s what to do. Grab a fine-grit sandpaper (start with 220 grit, then move to 400, then 800) and gently sand the bubbly area. You don’t need to sand all the way through the resin—just enough to remove the top layer where the bubble is. Once you’ve sanded out the bubble, wipe the surface clean with a lint-free cloth and isopropyl alcohol to remove all dust. Then, you can pour a thin layer of fresh resin over that spot, let it cure, and sand the entire piece smooth when it’s dry. I always recommend using the same resin brand for this—different resins have different curing times and hardness levels, so mixing brands can lead to adhesion issues later.

For larger, cured bubbles—say, a half-inch bubble on a resin tray that’s deep enough to see through—this takes a bit more work. You’ll need to use a Dremel tool with a small grinding bit to carefully carve out the bubble, making sure you don’t dig too deep and create a hole all the way through the project. Carve out the bubble until you have a smooth, concave space, then sand the edges of the carved area to make them sloped (this helps the new resin adhere instead of forming a ridge). Clean the area again with isopropyl alcohol, then mix a small batch of fresh resin (matching your original batch’s ratio exactly—too much hardener or resin will cause the new layer to cure unevenly) and fill the carved spot. Let it cure completely, then sand and polish the entire piece to blend the new layer with the old. I’ve done this fix on dozens of customer projects, and as long as you take your time, the patched spot is almost unnoticeable once finished.

Now, the biggest question: how do you prevent bubbles from forming in the first place? As a supplier, I see a lot of bubbles come from user error, not bad resin. Here are the most common mistakes I see, and how to avoid them. First, mixing resin and hardener incorrectly. Resin is a two-part system: part A is the resin, part B is the hardener, and they have to be mixed in the exact ratio specified on your bottle. If you add too much hardener, the chemical reaction speeds up, trapping air that can’t escape before it cures. If you add too little, the reaction is uneven, and you’ll get bubbles too. I always tell customers to measure both parts by volume, not by cups or spoons, because that’s imprecise. Use a digital scale—even a cheap kitchen scale works—to get an exact mix. I’ve had customers tell me, “I just guessed the ratio, and my resin came out bubbly” and that’s almost always the culprit.

Second, mixing too fast or too much air into the resin. When you stir, use a flat stick or a paint stirrer, and scrape the sides and bottom of your container to make sure all the resin and hardener are combined, but stir slowly—count to 30 while stirring, not 10. If you stir too fast, you’re whipping air into the mixture like cake batter, and those air bubbles will become trapped. For larger projects, I also recommend letting the mixed resin sit for 3 to 5 minutes after stirring—this is called “degassing,” and it lets any small air bubbles rise to the surface before you pour. That’s a step a lot of new makers skip, and it’s a game-changer.

Third, pouring resin in layers that are too thick. If you pour a layer of resin more than a quarter inch thick all at once, the exothermic reaction will get hot enough to trap air inside, and bubbles will form. Instead, pour thin layers—each no more than a quarter inch—and let each layer cure for 24 hours before pouring the next. For art pieces or small projects, this isn’t a big deal, but for tabletop casts or large resin projects, thick layers are a major bubble cause. Also, make sure your mold is clean and free of dust or moisture. Dust in the mold will mix with the resin, and moisture can create tiny bubbles as the resin cures. Wipe your mold with isopropyl alcohol before pouring, and let it dry completely—even a small drop of water can cause a bubble.

One other tip I share with all my customers: for clear resin projects, use a resin that’s formulated for low bubbling. Some resins are designed for high-volume pours and have additives that prevent air bubbles from forming during mixing and curing. When you’re choosing resin, read the product details—look for terms like “low-viscosity” or “self-degassing” if you’re prone to bubbles. As a supplier, I work with many makers who switched to our low-bubble resin and saw a 70% drop in bubbly projects, just because the resin was designed to release air easily.

Now, what about common myths I hear all the time? I can’t tell you how many times a customer has told me, “I tried heating the resin with a heat gun, and it made more bubbles!” The mistake here is using too high heat or getting too close to the surface. The heat gun should only be used to pop existing bubbles, not to heat the resin before pouring. Another myth: “ adding a little more hardener will make the resin cure faster and prevent bubbles.” No—too much hardener causes a faster reaction, which traps more bubbles, not less. I’ve seen this ruin dozens of projects, so I always warn people away from that hack. Finally, some people think that sanding and repouring is the only fix, but as I outlined earlier, small bubbles are easy to fix with a torch, and larger bubbles are manageable with a Dremel and fresh resin.

Whether you’re a hobbyist making resin keychains for friends or a small business owner producing resin jewelry, bubbly resin is a frustrating setback, but it’s rarely a dealbreaker. The key is to act fast if the resin is still green, be precise when mixing your resin and hardener, and take the time to degas before pouring. If you run into a bubble issue you can’t fix on your own, or if you’re looking for a low-bubble resin to help prevent problems in the first place, we’re here to help. We supply a range of acrylic resins for every project type, from small craft pieces to large structural casts, and we can advise you on the best resin for your needs, as well as troubleshooting tips for any bubbly mess you run into. To discuss your specific project or place an order, reach out to our team directly to get personalized support and product recommendations.

Glycol Ethers References:

  1. Resin Obsession. (2022). “How to Remove Bubbles from Resin.” Retrieved from resinobsession.com
  2. Modern Maker Supply Co. (2021). “Common Causes of Air Bubbles in Casting Resin.” Retrieved from modernmakersupply.com
  3. American Coatings Association. (2020). “Understanding Resin Curing Reactions for Casting Applications.” Retrieved from coatings.org
  4. Craft Resin. (2023). “A Guide to Repairing Cured Resin Projects.” Retrieved from craftresin.com

Henan GP Chemicals Co., Ltd.
Henan GP Chemicals Co., Ltd. is one of the most professional acrylic resin manufacturers and suppliers in China. We have world-leading production equipment and strong manufacturing capabilities. We warmly welcome you to buy bulk high quality acrylic resin made in China here from our factory.
Address: 29th Floor,The Cloud Center,NO.138 Ruida Road,Zhengzhou 450000,China
E-mail: info@gpcchem.com
WebSite: https://www.gpcchem.com/